7
14 13 5 20 56 12 38
0.2768 0.4955 0.0886 0.0225 0.0286 0.0863 0.0049 .0193
2.545
C

Data from;
  1. Glass substrates for AMLCD applications: Properties and implications",
     J.C. Lapp, presentation at SPIE 1997, corning document HP-Ab-03-4
  2. "influence of water on the diffusion of sodium in 1737 and in quartz glass"
     Lei Tian et. al., Cornell Center for Materials Research,
     National Science Foundation, DMR-9632275
Corning 1737 was introduced in 1994 as a replacement for Corning 7059.
In 2000 it was used for a large portion of the glass TFT market.
Corning Eagle 2000 began volume production in 2002 as a lighter weight
replacement for 1737.

The following composition comes from the Tian reference above.
9
14 8 13 5 20 56 12 38 33
0.2768 0.4730 0.0886 0.0225 0.0286 0.0863 0.0049 0.015 0.0043
2.545
PreSkeptic returns an array index error when it tries to 
build a table for this material. The 33 and 38 were combined
into 38 only with an adjusted weight fraction. Similarly,
the B was eliminated and the weight added to 8.
PreSkeptic builds with this composition.